4 Description of control M200 / M210 (optional)
4/14
4.9 Function sequence in operating modes
4.9.1 Explanation of signs and functions
Table :
Symbol Meaning
Press torch trigger
Release torch trigger
Shielding gas flowing
I
Welding power
Wire electrode is being discharged
Wire creep
The wire electrode does not reach the workpiece at full speed.
This facilitates reliable, spatter-free ignition.
Wire burn-back
Advantage: Prevents fusing of the wire electrode in the weld pool.
Wire back-burn set too high: large drops developing on the wire electrode result in
poor ignition properties or the wire electrode fusing onto the welding nozzle. Wire back-
burn set too low: Wire electrode fuses to the weld pool.
Gas pre-flows
Gas post-flows
The purpose of the gas post-flow is to prevent crater formation in the welding material
by keeping it surrounded with shielding gas until it solidifies.