4 Description of control M200 / M210 (optional)
4/12
4.8.3 No-power gas test
Key button for
gas test
This ensures a high standard of safety for the welder by
preventing accidental ignition of the arc.
4.8.4 Inching the wire electrode
Key button for
no-power inching
With the current off, the wire electrode can be inched into the
tube package without releasing gas.
4.8.5 Wire creep
Fig. 4/4; M200 control screen printing
The wire creep speed depends on the welding task (on the material, type of gas and wire diameter)
and is determined by characteristic curves.
Observe Fig. 4/4
The value for wire creep can be changed at a later time on the rear of the M200 controller (inside
the machine) on trimmer P3 (fully to the left = -20%, fully to the right = +20%; factory setting is
centre position). The changed wire feed speed will be available after the torch trigger is pressed
again.